Mon - Fri: 9:00 - 19:00
Grade : | AK4-1ch ( AK4-1ц ) |
Classification : | Aluminium wrought alloys |
Equivalent grades: | Go here |
Fe | Si | Ni | Ti | Al | Cu | Mg | Zn | Impurity |
---|---|---|---|---|---|---|---|---|
0.9 - 1.3 | 0.1 - 0.25 | 0.9 - 1.2 | 0.04 - 0.1 | 93.75 - 94.86 | 1.9 - 2.7 | 1.3 - 1.8 | max 0.1 | other, each 0.05; all 0.15 |
Comment: Al is a basis; the percentage of Al is given approximately.
T | E 10⁻⁵ | α 10⁶ | λ | ρ | C | R 10⁹ |
---|---|---|---|---|---|---|
Grade | MPa | 1/Grade | Watt/m·Grade | kg/m³ | J/(kg·Grade) | Ohm·m |
20 | 2800 |
Warning! Indicated both exact and nearest equivalents.
Inter |
ISO |
2618 |
B52 - Graded and shaped rolling
σB - Tensile strength [MPa]
σT - Yield stress [MPa]
δ5 - Specific elongation at fracture [%]
ψ - Reduction of area [%]
KCU - Impact strength [kJ/m²]
HB - Brinell hardness [MPa]
T - Test temperature [Grade]
E - Young modulus [MPa]
α - Coefficient of linear expansion (20° - T) [1/Grade]
λ - Thermal (heat) condition coefficient [Watt/(m·Grade)]
ρ - Density [kg/m³]
C - Specific heat (range 20° - T) [J/(kg·Grade)]
R - Electrical resistance [Ohm·m]