Mon - Fri: 9:00 - 19:00
Grade : | АK6 ( АК6 ) ( 1360 АКД6 ) |
Classification : | Aluminium wrought alloys |
Equivalent grades: | Go here |
Fe | Si | Mn | Ni | Ti | Al | Cu | Mg | Zn | Impurity |
---|---|---|---|---|---|---|---|---|---|
max 0.7 | 0.7 - 1.2 | 0.4 - 0.8 | max 0.1 | max 0.1 | 93.3 - 96.7 | 1.8 - 2.6 | 0.4 - 0.8 | max 0.3 | other, each 0.05; all 0.1 |
Assortment | Dimension | σb | σT | δ5 | ψ | KCU | Heat Treatment |
---|---|---|---|---|---|---|---|
- | mm | MPa | MPa | % | - | kJ/m² | - |
Pipe, GOST 18482-79 | 285-355 | 8-10 | Quenching and artificial aging | ||||
Bar, GOST 21488-97 | 355 | 12 | Quenching and artificial aging | ||||
Bar, GOST 51834-2001 | 390-430 | 275-325 | 10 | Quenching and artificial aging | |||
Profile, GOST 8617-81 | 353 | 12 | Quenching and artificial aging |
T | E 10⁻⁵ | α 10⁶ | λ | ρ | C | R 10⁹ |
---|---|---|---|---|---|---|
Grade | MPa | (1/Grade) | (Watt/m·Grade) | (kg/m³) | (J/kg·Grade) | (Ohm·m) |
20 | 0.72 | 21.4 | 180 | 2750 | 838 | 41 |
100 | - | - | - | - | - | - |
USA | Japan | France | England | European | Italy | Poland | Czechia |
---|---|---|---|---|---|---|---|
- | JIS | AFNOR | BS | EN | UNI | PN | CSN |
2117 | 2117 | A-U2G | L86 | ENAW-AlCuMg0.5 | P-AlCu2.5MgSi | AlCu2SiMn | 424206 |
σB - Tensile strength [MPa]
σT - Yield stress [MPa]
δ5 - Specific elongation at fracture [%]
ψ - Reduction of area [%]
KCU - Impact strength [kJ/m²]
HB - Brinell hardness [MPa]
T - Test temperature [Grade]
E - Young modulus [MPa]
α - Coefficient of linear expansion (20° - T) [1/Grade]
λ - Thermal (heat) condition coefficient [Watt/(m·Grade)]
ρ - Density [kg/m³]
C - Specific heat (range 20° - T) [J/(kg·Grade)]
R - Electrical resistance [Ohm·m]