Mon - Fri: 9:00 - 19:00
Brand : | TS6 |
Classification : | Titanium wrought alloy |
Application: | for the production of cavitation-resistant products; pseudo β structure class |
Foreign analogues: | No data |
GOST -27265 - 87
Cr | M | V | You | Al |
---|---|---|---|---|
10 - 11 | 4 - 5 | 6 - 6 | 75 - 77 | 3 - 3 |
Note: Ti is the basis; Ti percentage is approximate.
Mechanical properties at T=20 o C of material TS6.
Assortment | Size | For example. | σin | σT | δ5 | ψ | KCU | Thermal processing |
---|---|---|---|---|---|---|---|---|
- | mm | - | MPa | MPa | % | % | kJ/m² | - |
Sheet | 1580-1635 | 1520-1590 | 5.5-6 | Hardening and aging |
Hardness TC6 after quenching and aging, Sheet | HB 10 -1 = 341 - 444 MPa |
σin - Tensile strength [MPa]
σT - Yield stress [MPa]
δ5 - Specific elongation at fracture [%]
ψ - Reduction of area [%]
KCU - Impact strength [kJ/m²]
HB - Brinell hardness [MPa]
T - Test temperature [Grade]
E - Young modulus [MPa]
α - Coefficient of linear expansion (20° - T) [1/Grade]
λ - Thermal (heat) condition coefficient [Watt/(m·Grade)]
ρ - Density [kg/m³]
C - Specific heat (range 20° - T) [J/(kg·Grade)]
R - Electrical resistance [Ohm·m]